Advantica® F Heat
A pre-finished steel product with excellent heat resistance
Characteristics
• Very good heat performance
• Smooth surface appearance
Substrates available
• Hot-dip galvanised to EN 10346
• Cold reduced to EN 10130
Options
• Alternative backing coats available
• Protective film
Advantica® F Heat
Typical properties | | | Test specification |
Nominal coating thickness |
μm |
25 |
EN 13523-1 |
Specular gloss (60°) |
GU |
50-60
|
EN 13523-2 |
Adhesion on bending |
T |
0 |
EN 13523-7 |
Flexibility (minimum bend radius) |
T |
3 |
EN 13523-7 |
Pencil hardness |
|
F |
EN 13523-4 |
Scratch resistance |
g |
>1800 |
EN 13523-12 |
Abrasion resistance (Taber, 250 rev. 1kg, CS10 wheels) |
mg |
<30 |
EN 13523-16 |
Corrosion resistance: Neutral salt spray
|
Hours |
360 |
EN 13523-16 |
Corrosion resistance: Humidity resistance
|
Hours |
1000 |
EN 13523-26 |
Resistance to accelerated ageing by use of heat |
|
Delta E <0,5 at 200 hours 120oC Delta E <1 at 3 hrs 180oC Flexibility: max 1T loss after both ageings
|
EN 13523-13 |
Notes
The figures contained in this table are typical properties and do not constitute a
specification. If forming pre-finished steel below 16°C please consult Tata Steel for further
information.
Corrosion and humidity performance subject to specification such as minimal metallic coating weight.